Xinhai Group

Armenia 1,500t/d Copper-Lead-Zinc Mineral Processing Plant
CASES

Armenia 1,500t/d Copper-Lead-Zinc Mineral Processing Plant

The deposit was characterized by carbonatite. The raw ore consisted of two metallic minerals (galena and blende) and one gangue mineral (diopside). It had a grade of 5.61g/t.

Xinhai Solution

01

Two-stage closed-circuit crushing-one-stage self-grinding and lead roughing concentrates regrinding-differential flotation-two-stage dewatering

02

After the raw ore was ground, lead concentrates were produced through one-stage roughing, three-stage scavenging and three-stage concentration, with a recovery of 90.49%.

03

The dehydration operation was carried out by disc vacuum filter, and the dehydration rate was more than 95%.

Project Result

Armenia 1,500t/d Copper-Lead-Zinc Mineral Processing Plant

The raw ore had a grade of 5.61g/t, and lead concentrates (78.85g/t) were produced with a recovery of 90.49%. The project was well received by the client.

Project Site

Armenia 1,500t/d Copper-Lead-Zinc Mineral Processing Plant
Armenia 1,500t/d Copper-Lead-Zinc Mineral Processing Plant
Armenia 1,500t/d Copper-Lead-Zinc Mineral Processing Plant